Only .25 pellet at ~40ft/lb punch through this relatively thick flashlight tube. Shooting SLN 6061 Sample tomorrow and this is quite discouraging. At first I was expecting it to survive .380 but now I am happy it lived .22LR and leave the 7075 for the .380.
.22lr is about 90ft/lb
.380 is about 150ft/lb
.32 HR Magnum 220ft/lb
9mm 320ft/lb
.327 Magnum 450ft/lb
Absolutely beautiful, the machining is so very well done. I love the polished look, is there a clear anodize on that? Tip of the cap to you on pulling the entire project together, from inception to realizing the final piece, you should be very proud!!
I’m with DBSAR, am eagerly awaiting release of the group buy LT1’s, would love to see an LT1vn
Congratulations again, and thank you for such thorough detailed releases of your step by step processes, is quite fascinating to follow. Keep it up.
No clear anodized yet. Just Raw 7075. I plan just to keep these few Raw. Will provide some clear anodized in the next run instead.
Thank you for the support!