thefreeman
(thefreeman)
358
What alloy is 158° ?
I’ve used the three main ones, SnPb, SAC (SnAgCu) and BiSnAg, all from Chipquik.
- SnPb flows the best and is the easiest to use, but is leaded of course.
- SAC is the worst IMO, doesn’t flow well i.e. tends to make bridges if the paste application isn’t perfect, the high temp requires good equipment and limits the number of reflow and working time. Touching up joints, which is often needed, is difficult with a small iron tip without some sort of preheating (hotplate).
- BiSn doesn’t flow as well as SnPb but better than SAC, the low temp is great if your equipment has trouble heating up to SAC temp. It’s the easy lead-free option.
It makes poor joints if mixed with SnPb, so it’s better to also have BiSn wire when using BiSn paste.
1 Thank