Scratch test to test out the HAIII anodization

Firstly a flourite rock. The head section was scratched with the rock

The resultant marks were simply removed with wiping

Next a harder rock, this time a Garnet. This has a MOH rating of around 7, diamond is 10.

The marks made on the head were not as noticable as those form the flourite.

After some wiping almost all of the marks have been removed. You can barely see the scratches on the head section below.

Overall an excellent result for the anodization. It’s of a high standard.

Thank you Rolz for the hardness testing :+1: